Pure Nickel Wire is a high-quality metal wire made of highly pure nickel material. The material grade is usually Ni200 or Ni201, with a purity of over 99.5%, ensuring the excellent performance of the material.
Pure Nickel Wire has excellent corrosion resistance and can maintain stability for long periods of time in harsh environments. It exhibits excellent corrosion resistance to many chemicals, acids, alkalis, and corrosive gases, making it an ideal choice for corrosion resistant equipment and chemical treatment systems.
Specification
Grade | Ni+Co | Cu | Si | Mn | C | Mg | S | P | Fe |
N4 | 99.9 | ≤0.015 | ≤0.03 | ≤0.002 | ≤0.01 | ≤0.01 | ≤0.001 | ≤0.001 | ≤0.04 |
N6 | 99.5 | 0.10 | 0.10 | 0.05 | 0.10 | 0.10 | 0.005 | 0.002 | 0.10 |
Ni201 | ≥99.9 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.02 | / | ≤0.01 | / | ≤0.40 |
Ni200 | ≥99.6 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.15 | / | ≤0.01 | / | ≤0.40 |
Physical Data | |
Density | 8.89g/cm3 |
Specific Heat | 0.109(456 J/kg.ºC) |
Electrical Resistivity | 0.096×10-6ohm.m |
Melting Point | 1435-1446ºC |
Thermal Conductivity | 70.2 W/m-K |
Mean Coeff Thermal Expansion | 13.3×10-6m/m.ºC |
Typical Mechanical Properties | |
Mechanical Properties | Nickel 200 |
Tensile Strength | 462 Mpa |
Yield Strength | 148 Mpa |
Elongation | 47% |
![]() |
|
![]() |
![]() |
MOQ: | 1KG |
Price: | 5 - 99 kilograms US$45.00 |
Standard Packaging: | Spool package with Carton box, Coil package with polybag, |
Delivery Period: | 7-25 days |
Payment Method: | L/C, T/T, Western Union, MoneyGram |
Supply Capacity: | 300 tons per month |
Pure Nickel Wire is a high-quality metal wire made of highly pure nickel material. The material grade is usually Ni200 or Ni201, with a purity of over 99.5%, ensuring the excellent performance of the material.
Pure Nickel Wire has excellent corrosion resistance and can maintain stability for long periods of time in harsh environments. It exhibits excellent corrosion resistance to many chemicals, acids, alkalis, and corrosive gases, making it an ideal choice for corrosion resistant equipment and chemical treatment systems.
Specification
Grade | Ni+Co | Cu | Si | Mn | C | Mg | S | P | Fe |
N4 | 99.9 | ≤0.015 | ≤0.03 | ≤0.002 | ≤0.01 | ≤0.01 | ≤0.001 | ≤0.001 | ≤0.04 |
N6 | 99.5 | 0.10 | 0.10 | 0.05 | 0.10 | 0.10 | 0.005 | 0.002 | 0.10 |
Ni201 | ≥99.9 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.02 | / | ≤0.01 | / | ≤0.40 |
Ni200 | ≥99.6 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.15 | / | ≤0.01 | / | ≤0.40 |
Physical Data | |
Density | 8.89g/cm3 |
Specific Heat | 0.109(456 J/kg.ºC) |
Electrical Resistivity | 0.096×10-6ohm.m |
Melting Point | 1435-1446ºC |
Thermal Conductivity | 70.2 W/m-K |
Mean Coeff Thermal Expansion | 13.3×10-6m/m.ºC |
Typical Mechanical Properties | |
Mechanical Properties | Nickel 200 |
Tensile Strength | 462 Mpa |
Yield Strength | 148 Mpa |
Elongation | 47% |
![]() |
|
![]() |
![]() |