AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components

AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components

MOQ: 30 Kg
Price: Negotiable
Standard Packaging: Spool Carton box, Coil package with polybag,then in woodencase
Delivery Period: 20~40 Days
Payment Method: L/C, T/T, Western Union, MoneyGram
Supply Capacity: 300 tons per month
Detail Information
Place of Origin
China
Brand Name
Victory
Certification
ISO9001 ROHS
Model Number
Inconel 718
Name:
AMS 5596 ASTM B670 Superalloy Nickel Alloy 718 Inconel 718 Strip For Aerospace Components
Material:
Nickel Chromium Iron
Ni (Min):
50~55%
Density:
8.24 G/cm3
Melting Point:
1260-1320°C
Elongation (≥ %):
25 %
Thermal Conductivity:
15.9 W/m·K
Finishing:
Bright,Oxided, Acid White
Application:
Construction, Industry Oil, Piping Systems
Yield Strength:
550MPa
Tensile Strength:
910 MPa
Hardness:
≤ 363 HB
Standard:
ASTM, ASME
Size:
6~200mm
Shape:
Round, Square, Flat
Highlight:

Aerospace Components Inconel 718 Strip

,

ASTM B670 Inconel 718 Strip

,

AMS 5596 Inconel 718 Strip

Product Description

Advantages of Inconel 718 Strips



High Strength-to-Weight Ratio: Provides durability without adding excessive weight.
Excellent Fabricability: Can be easily machined and formed into complex shapes.
Resistance to Oxidation and Corrosion: Ensures longevity in challenging environments.

 

 

Applications of Inconel 718 Strips


Aerospace Components

Thrust Reversers: Used in thrust reversers for jet engines, where high-temperature resistance and strength are essential.
Structural Components: Fabricated into various structural parts that require lightweight yet strong materials.
Oil and Gas Industry

Downhole Equipment: Employed in valves, fittings, and other components exposed to harsh environments.
Subsea Applications: Ideal for use in subsea pipelines and connectors due to its excellent corrosion resistance.
Nuclear Applications

Fuel Rods and Structural Supports: Used in nuclear reactors where materials must withstand extreme conditions.
Marine Applications

Components in Marine Engines: Suitable for various parts exposed to seawater, where corrosion resistance is vital.
High-Performance Engineering

Fasteners and Bolts: Can be used to manufacture bolts and fasteners that require superior mechanical properties.
Heat Exchangers

Heat Exchanger Tubes: Utilized in heat exchangers where high temperatures and corrosive fluids are present.

 

 

Parameter:

Chemical Properties of Inconel 718

 

Nickel (plus Cobalt) .......................................................50.00-55.00

Chromium......................................................................17.00-21.00

Iron .....................................................................................Balance

Niobium (plus Tantalum)....................................................4.75-5.50

Molybdenum .....................................................................2.80-3.30

Titanium.............................................................................0.65-1.15

Aluminum ..........................................................................0.20-0.80

Cobalt ...............................................................................1.00 max.

Carbon..............................................................................0.08 max.

Manganese .......................................................................0.35 max.

Silicon ...............................................................................0.35 max.

Phosphorus.....................................................................0.015 max.

Sulfur...............................................................................0.015 max.

Boron ..............................................................................0.006 max.

Copper..............................................................................0.30 max

 

 

Density 8.19g/cm³ 0.296 lb/in³
Melting point 1260-1336 2437°F

 

SPECIFICATIONS
 
Form
  ASTM
Rod,bar and wire
B 166
Plate,sheet and strip
B 168, B 906
Seamless pipe and tube
B 167, B 829
Welded pipe
B 517, B775
Fitting 
B 366
Billet and bar for reforging
B 472
Forging
B 564

 

Inconel series

Steel grade
Inconel 600
Inconel 601
Inconel 625
Inconel 718
Inconel 725
Inconel X-750
Corresponding brand
N06600/2.4816/1Cr15Ni75Fe8/NS312/CY40
N06601/2.4851/1Cr23Ni60Fe13AI/NS313
N06625/2.4856/0Cr20Ni65Mo10bN4/NS336
N07718/2.4668/GH4169
N07725
N07750/2.4669/GH4145
Chemical composition%
C≤
0.150
0.100
0.100
0.080
0.030
0.080
Mn≤
1.00
1.00
0.50
0.35
0.35
1.00
P≤
/
/
0.015
0.015
0.015
/
S≤
0.015
0.015
0.015
0.015
0.010
0.010
Si≤
0.50
0.50
0.50
0.35
0.20
0.50
Cr≤
14.0-17.0
21.0-25.0
20.0-23.0
17.0-21.0
19.0-22.5
14.0-17.0
Ni≤
≥72.0
58.0-63.0
≥58.0
55.0-59.0
55.0-59.0
≥70
Mo
/
/
8.0-10.0
2.8-3.3
7.0-9.5
/
Cu
≤0.50
≤1.50
/
≤0.30
/
≤0.50
N
/
/
/
 
/
/
Nb
/
/
3.15-4.15
4.75-5.50
2.75-4.00
0.70-1.20
other
Fe:6.0-10.0
Al:1.0-1.7
Co:≤1.0Ai:≤0.40Tr:0.40Fe:≤5.0
AI:0.20-0.80Ti:0.65-1.15B≤0.006
Tr:1.0-1.7AI≤0.35
Co:≤1.0 AI:0.4-1.0Tr:0.25-2.75Fe:5.0-9.0

 

 

Customize size as below

 

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

 

 

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 0AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 1AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 2AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 3AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 4

 

 

 

 

 
Products
PRODUCTS DETAILS
AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components
MOQ: 30 Kg
Price: Negotiable
Standard Packaging: Spool Carton box, Coil package with polybag,then in woodencase
Delivery Period: 20~40 Days
Payment Method: L/C, T/T, Western Union, MoneyGram
Supply Capacity: 300 tons per month
Detail Information
Place of Origin
China
Brand Name
Victory
Certification
ISO9001 ROHS
Model Number
Inconel 718
Name:
AMS 5596 ASTM B670 Superalloy Nickel Alloy 718 Inconel 718 Strip For Aerospace Components
Material:
Nickel Chromium Iron
Ni (Min):
50~55%
Density:
8.24 G/cm3
Melting Point:
1260-1320°C
Elongation (≥ %):
25 %
Thermal Conductivity:
15.9 W/m·K
Finishing:
Bright,Oxided, Acid White
Application:
Construction, Industry Oil, Piping Systems
Yield Strength:
550MPa
Tensile Strength:
910 MPa
Hardness:
≤ 363 HB
Standard:
ASTM, ASME
Size:
6~200mm
Shape:
Round, Square, Flat
Minimum Order Quantity:
30 Kg
Price:
Negotiable
Packaging Details:
Spool Carton box, Coil package with polybag,then in woodencase
Delivery Time:
20~40 Days
Payment Terms:
L/C, T/T, Western Union, MoneyGram
Supply Ability:
300 tons per month
Highlight

Aerospace Components Inconel 718 Strip

,

ASTM B670 Inconel 718 Strip

,

AMS 5596 Inconel 718 Strip

Product Description

Advantages of Inconel 718 Strips



High Strength-to-Weight Ratio: Provides durability without adding excessive weight.
Excellent Fabricability: Can be easily machined and formed into complex shapes.
Resistance to Oxidation and Corrosion: Ensures longevity in challenging environments.

 

 

Applications of Inconel 718 Strips


Aerospace Components

Thrust Reversers: Used in thrust reversers for jet engines, where high-temperature resistance and strength are essential.
Structural Components: Fabricated into various structural parts that require lightweight yet strong materials.
Oil and Gas Industry

Downhole Equipment: Employed in valves, fittings, and other components exposed to harsh environments.
Subsea Applications: Ideal for use in subsea pipelines and connectors due to its excellent corrosion resistance.
Nuclear Applications

Fuel Rods and Structural Supports: Used in nuclear reactors where materials must withstand extreme conditions.
Marine Applications

Components in Marine Engines: Suitable for various parts exposed to seawater, where corrosion resistance is vital.
High-Performance Engineering

Fasteners and Bolts: Can be used to manufacture bolts and fasteners that require superior mechanical properties.
Heat Exchangers

Heat Exchanger Tubes: Utilized in heat exchangers where high temperatures and corrosive fluids are present.

 

 

Parameter:

Chemical Properties of Inconel 718

 

Nickel (plus Cobalt) .......................................................50.00-55.00

Chromium......................................................................17.00-21.00

Iron .....................................................................................Balance

Niobium (plus Tantalum)....................................................4.75-5.50

Molybdenum .....................................................................2.80-3.30

Titanium.............................................................................0.65-1.15

Aluminum ..........................................................................0.20-0.80

Cobalt ...............................................................................1.00 max.

Carbon..............................................................................0.08 max.

Manganese .......................................................................0.35 max.

Silicon ...............................................................................0.35 max.

Phosphorus.....................................................................0.015 max.

Sulfur...............................................................................0.015 max.

Boron ..............................................................................0.006 max.

Copper..............................................................................0.30 max

 

 

Density 8.19g/cm³ 0.296 lb/in³
Melting point 1260-1336 2437°F

 

SPECIFICATIONS
 
Form
  ASTM
Rod,bar and wire
B 166
Plate,sheet and strip
B 168, B 906
Seamless pipe and tube
B 167, B 829
Welded pipe
B 517, B775
Fitting 
B 366
Billet and bar for reforging
B 472
Forging
B 564

 

Inconel series

Steel grade
Inconel 600
Inconel 601
Inconel 625
Inconel 718
Inconel 725
Inconel X-750
Corresponding brand
N06600/2.4816/1Cr15Ni75Fe8/NS312/CY40
N06601/2.4851/1Cr23Ni60Fe13AI/NS313
N06625/2.4856/0Cr20Ni65Mo10bN4/NS336
N07718/2.4668/GH4169
N07725
N07750/2.4669/GH4145
Chemical composition%
C≤
0.150
0.100
0.100
0.080
0.030
0.080
Mn≤
1.00
1.00
0.50
0.35
0.35
1.00
P≤
/
/
0.015
0.015
0.015
/
S≤
0.015
0.015
0.015
0.015
0.010
0.010
Si≤
0.50
0.50
0.50
0.35
0.20
0.50
Cr≤
14.0-17.0
21.0-25.0
20.0-23.0
17.0-21.0
19.0-22.5
14.0-17.0
Ni≤
≥72.0
58.0-63.0
≥58.0
55.0-59.0
55.0-59.0
≥70
Mo
/
/
8.0-10.0
2.8-3.3
7.0-9.5
/
Cu
≤0.50
≤1.50
/
≤0.30
/
≤0.50
N
/
/
/
 
/
/
Nb
/
/
3.15-4.15
4.75-5.50
2.75-4.00
0.70-1.20
other
Fe:6.0-10.0
Al:1.0-1.7
Co:≤1.0Ai:≤0.40Tr:0.40Fe:≤5.0
AI:0.20-0.80Ti:0.65-1.15B≤0.006
Tr:1.0-1.7AI≤0.35
Co:≤1.0 AI:0.4-1.0Tr:0.25-2.75Fe:5.0-9.0

 

 

Customize size as below

 

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

 

 

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 0AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 1AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 2AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 3AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components 4

 

 

 

 

 
Sitemap |  Privacy Policy | China Good Quality Nichrome Alloy Supplier. Copyright © 2023-2025 Changzhou Victory Technology Co., Ltd . All Rights Reserved.