Products
PRODUCTS DETAILS
Home > Products >
Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe

Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe

MOQ: 30 Kg
Price: Negotiable
Standard Packaging: Inconel 600 rod packed in Spool Carton box, Coil package with polybag,then in woodencase
Delivery Period: 20~40 Days
Payment Method: L/C, T/T, Western Union, MoneyGram
Supply Capacity: 300 tons per month
Detail Information
Place of Origin
China
Brand Name
Victory
Certification
ISO9001 ROHS
Model Number
Inconel 600
Name:
Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe
Material:
Nickel Chromium Iron
Ni (Min):
72%
Density:
8.47 G/cm3
Melting Point:
1,370-1,425°C
Elongation (≥ %):
30 %
Thermal Conductivity:
15.9 W/m·K
Finishing:
Bright,Oxided
Application:
Construction, Industry Oil, Piping Systems
Yield Strength:
240 MPa
Tensile Strength:
550 MPa
Hardness:
≤ 160 HB
Standard:
ASTM, ASME
Size:
6~500mm
Shape:
Round, Square, Seamless, Welded
Highlight:

welded pipe inconel 600 seamless tube

,

Corrosion Resistant Inconel 600 Seamless Tube

,

Superalloy Inconel 600 Seamless Tube

Product Description

The performance characteristics of Inconel 600 tube


Excellent corrosion resistance: Inconel 600 has outstanding corrosion resistance, capable of withstanding many corrosive environments, such as the chemical industry, marine environments, and high temperature environments.

High temperature resistance: Inconel 600 tubing can be used for long-term service at temperatures up to 1100°C, making it suitable for high temperature industrial applications.

Good mechanical properties: Inconel 600 tubing has relatively high strength, toughness and fatigue performance, able to withstand high mechanical stresses.

Low thermal expansion coefficient: Inconel 600 has a low thermal expansion coefficient, which is beneficial for maintaining dimensional stability of the tubing under temperature variations.

Excellent oxidation resistance: Inconel 600 tubing can form a dense oxide layer at high temperatures, effectively preventing further oxidation of the inner metal.

 

The differences between seamless and welded tubing/pipes


Manufacturing process:
Seamless tubes are produced by piercing a solid billet or ingot and then further reducing the diameter and increasing the length.
Welded tubes are formed by bending a flat metal sheet/strip and joining the edges together using a welding process.


Structural integrity:
Seamless tubes have a more uniform and continuous structure without any welded seams.
Welded tubes have a welded joint along the length, which can be a potential weak point.


Surface quality:
Seamless tubes generally have a smoother and more uniform surface finish.
Welded tubes may have some surface irregularities along the weld line.


Strength and toughness:
Seamless tubes typically have higher strength and impact toughness compared to welded tubes.
The weld joint in welded tubes can be a point of weakness.


Cost and availability:
Seamless tubes are generally more expensive to manufacture than welded tubes.
Welded tubes are often more readily available and can be produced in a wider range of sizes and shapes.

 

 

 

Parameter:

Chemical Properties of Inconel 600

 

C Cr Ni+Co Al Ti Fe Nb+Ta Mn Si P S Cu
≤0.15 14.0~17.0 ≥72 ≤0.35 ≤0.50 6.0~10.0 ≤1.0 ≤1.0 ≤0.5 ≤0.04 ≤0.015 ≤0.5

 

ITEM θ/℃ TENSIE STRENGTH HBS
σb/MPa σP0.2/MPa δ5/% φ/%
BAR/ROD 20 ≥585 ≥240 ≥30 - 134~217
RING 20 ≥520 ≥205 ≥35 - ≥187
HOT ROLL PLATE 20 ≥550 ≥240 ≥35 ≥40 -
900 ≥95 ≥45 ≥40 ≥50 -
COLD ROLLED SHEET 20 ≥550 ≥240 ≥30 - -
900 ≥90 ≥40 ≥60 - -
COLD ROLLED SHEET 20 ≥550 ≥200 ≥30 - -
STRIP 20 ≥550 ≥240 ≥30 - -
WIRE 20       - HV≤151

 

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

 

 

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe 0Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe 1Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe 2

 

 

 

 

 

Products
PRODUCTS DETAILS
Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe
MOQ: 30 Kg
Price: Negotiable
Standard Packaging: Inconel 600 rod packed in Spool Carton box, Coil package with polybag,then in woodencase
Delivery Period: 20~40 Days
Payment Method: L/C, T/T, Western Union, MoneyGram
Supply Capacity: 300 tons per month
Detail Information
Place of Origin
China
Brand Name
Victory
Certification
ISO9001 ROHS
Model Number
Inconel 600
Name:
Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe
Material:
Nickel Chromium Iron
Ni (Min):
72%
Density:
8.47 G/cm3
Melting Point:
1,370-1,425°C
Elongation (≥ %):
30 %
Thermal Conductivity:
15.9 W/m·K
Finishing:
Bright,Oxided
Application:
Construction, Industry Oil, Piping Systems
Yield Strength:
240 MPa
Tensile Strength:
550 MPa
Hardness:
≤ 160 HB
Standard:
ASTM, ASME
Size:
6~500mm
Shape:
Round, Square, Seamless, Welded
Minimum Order Quantity:
30 Kg
Price:
Negotiable
Packaging Details:
Inconel 600 rod packed in Spool Carton box, Coil package with polybag,then in woodencase
Delivery Time:
20~40 Days
Payment Terms:
L/C, T/T, Western Union, MoneyGram
Supply Ability:
300 tons per month
Highlight

welded pipe inconel 600 seamless tube

,

Corrosion Resistant Inconel 600 Seamless Tube

,

Superalloy Inconel 600 Seamless Tube

Product Description

The performance characteristics of Inconel 600 tube


Excellent corrosion resistance: Inconel 600 has outstanding corrosion resistance, capable of withstanding many corrosive environments, such as the chemical industry, marine environments, and high temperature environments.

High temperature resistance: Inconel 600 tubing can be used for long-term service at temperatures up to 1100°C, making it suitable for high temperature industrial applications.

Good mechanical properties: Inconel 600 tubing has relatively high strength, toughness and fatigue performance, able to withstand high mechanical stresses.

Low thermal expansion coefficient: Inconel 600 has a low thermal expansion coefficient, which is beneficial for maintaining dimensional stability of the tubing under temperature variations.

Excellent oxidation resistance: Inconel 600 tubing can form a dense oxide layer at high temperatures, effectively preventing further oxidation of the inner metal.

 

The differences between seamless and welded tubing/pipes


Manufacturing process:
Seamless tubes are produced by piercing a solid billet or ingot and then further reducing the diameter and increasing the length.
Welded tubes are formed by bending a flat metal sheet/strip and joining the edges together using a welding process.


Structural integrity:
Seamless tubes have a more uniform and continuous structure without any welded seams.
Welded tubes have a welded joint along the length, which can be a potential weak point.


Surface quality:
Seamless tubes generally have a smoother and more uniform surface finish.
Welded tubes may have some surface irregularities along the weld line.


Strength and toughness:
Seamless tubes typically have higher strength and impact toughness compared to welded tubes.
The weld joint in welded tubes can be a point of weakness.


Cost and availability:
Seamless tubes are generally more expensive to manufacture than welded tubes.
Welded tubes are often more readily available and can be produced in a wider range of sizes and shapes.

 

 

 

Parameter:

Chemical Properties of Inconel 600

 

C Cr Ni+Co Al Ti Fe Nb+Ta Mn Si P S Cu
≤0.15 14.0~17.0 ≥72 ≤0.35 ≤0.50 6.0~10.0 ≤1.0 ≤1.0 ≤0.5 ≤0.04 ≤0.015 ≤0.5

 

ITEM θ/℃ TENSIE STRENGTH HBS
σb/MPa σP0.2/MPa δ5/% φ/%
BAR/ROD 20 ≥585 ≥240 ≥30 - 134~217
RING 20 ≥520 ≥205 ≥35 - ≥187
HOT ROLL PLATE 20 ≥550 ≥240 ≥35 ≥40 -
900 ≥95 ≥45 ≥40 ≥50 -
COLD ROLLED SHEET 20 ≥550 ≥240 ≥30 - -
900 ≥90 ≥40 ≥60 - -
COLD ROLLED SHEET 20 ≥550 ≥200 ≥30 - -
STRIP 20 ≥550 ≥240 ≥30 - -
WIRE 20       - HV≤151

 

Shape
Size(mm)
WIre
0.5-7.5
Rod/Bar
8.0-200
Strip
(0.5-2.5)*(5-180)
Tube
custom made
Plate
custom made

 

 

contact us

email:victory@dlx-alloy.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe 0Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe 1Excellent Corrosion Resistant Superalloy Nickel Chrome Inconel 600 Seamless Tube Welded Pipe 2

 

 

 

 

 

Sitemap |  Privacy Policy | China Good Quality Nichrome Alloy Supplier. Copyright © 2023-2025 Changzhou Victory Technology Co., Ltd . All Rights Reserved.